Hi, Dave,

I didn't change any other parameters (only final thickness and rate of deposition) in the program.
When I did Al2O3 this morning, it works well. Then I just switch to Ag and appear the problem I reported.

Best.
Zhuoxian

----- 原始邮件 -----
发件人: "David A Lubelski" <lubelski at purdue.edu>
收件人: "Zhuoxian Wang" <wang1973 at purdue.edu>
抄送: "Jingjing Liu (liu175 at purdue.edu)" <liu175 at purdue.edu>, "Ronald K Reger" <rreger at purdue.edu>, "Dimitrios Peroulis" <dperouli at purdue.edu>, leybold-list at ecn.purdue.edu
发送时间: 星期二, 2014年 7 月 01日 下午 3:17:56
主题: RE: Leybold

Zhuoxian,
The reason the system did not work for you was the programming had been changed in the controller.  The only two settings you need to change are the final thickness and rate of deposition.  As you were trained, there is no reason to change any other setting. Doing so leads to reports of the system either having problems or being down, which is not the case. If you would like another training session, please let me know and I will sit down with you this week for additional training/clarification.
 Please remember, I am here to assist you in any way possible to help make your research needs are met.
Thank you,
Dave Lubelski

-----Original Message-----
From: Zhuoxian Wang [mailto:wang1973 at purdue.edu] 
Sent: Tuesday, July 01, 2014 12:27 PM
To: Lubelski, David A
Subject: Leybold

Hi, Dave,

When I use Leybold to deposit silver, it can not read the deposition rate after open the shutter.
I was OK when I deposit Al2O3.

Would you mind have a look at it.